STRENGTH DEVELOPMENT AND MODULUS OF ELASTICITY IN RELATION TO STORING

FESTIGKEITSENTWICKLUNG UND E-MODUL IN ABHAENGIGKEIT VON DER LAGERUNG

Where concrete units are not protected from drying out for at least three days after casting, strength losses must be expected. Even after three days, the increase in modulus of elasticity after 28 days is significantly smaller than in the case of concrete which has not been allowed to dry out. /TRRL/

  • Authors:
    • Nischer, P
  • Publication Date: 1977

Language

  • German

Media Info

  • Features: Figures; References;
  • Pagination: p. 140-144