BATTER AT CWR WELDS? HERE'S HOW TO MAKE REPAIRS

Some continuous welded rail develops battered butt weld areas which gradually increase in length and depth, depending on wheel loads and speeds. With an eight-step procedure, using a core wire with a semi-automatic wire-feed welding unit, deposits of the proper hardness can be applied when used in conjunction with a controlled pre-heat and post-heat procedure.