PROPERTIES OF GRANULATED BLAST-FURNACE SLAG CEMENT CONCRETE

In this study, moderate heat portland cement, in which the fineness is 300 m sq/kg, and granulated blast furnace slag, in which the fineness is 300, 400, 500 and 600 m sq/kg. were made. The slag content in cement is 50, 60, 70, and 80%. Tests for settling and heat of hydration in cement and for setting, compressive strength , freezing and thawing, adiabatic temperature rise, corbonation, and drying shrinkdge in concrete were carried out. The details of the study are described, and the results are presented and discussed.

Language

  • English

Media Info

  • Features: Figures; References; Tables;
  • Pagination: p. 1367-83
  • Serial:
    • Volume: 2

Subject/Index Terms

Filing Info

  • Accession Number: 00624400
  • Record Type: Publication
  • Report/Paper Numbers: SP-132
  • Files: TRIS
  • Created Date: Oct 26 1993 12:00AM