TEST ON MARINE REDUCTION GEAR BY MEANS OF A LARGE TEST RIG

Results of load tests on large reduction gears tested on a testing machine having a centre distance of 720mm are described. Non-modified shaved gears failed after K=350 psi load run at 100 million cycles. Modified shaved gears failed after K=400 psi load run at 50 million cycles. In addition the paper deals with the tooth load distributions by measuring the stress in the root fillet, temperature difference between gear and pinion, and temperature distributions on the tooth face. Order from NSFI as No. 22437.

  • Corporate Authors:

    Marine Engineering Society in Japan

    Osaka Building, 1-2-2 Uchisaiwai-Cho, Chiyoda-Ku
    Tokyo 100,   Japan 
  • Authors:
    • Yamakura, Y
    • Okajima, M
    • Seto, T
  • Publication Date: 1980

Media Info

Subject/Index Terms

Filing Info

  • Accession Number: 00331991
  • Record Type: Publication
  • Source Agency: Ship Research Institute of Norway
  • Files: TRIS
  • Created Date: Jun 12 1981 12:00AM