PRIMERS FOR SPRAYED ALUMINUM AND ZINC COATINGS ON STEEL

EXPOSURE TRIALS OF UP TO 8 YEARS DURATION HAVE BEEN CONDUCTED ON PRIMING PAINTS FOR SPRAYED ALUMINIUM AND SPRAYED ZINC EXPOSED TO THE ATMOSPHERE. MOST OF THE PAINTS TESTED PERFORMED WELL AND THE CHEMICAL COMPOSITION CHOSEN FOR THE PRIMER IS THEREFORE NOT CONSIDERED CRITICAL, ALTHOUGH ITS PHYSICAL CHARACTERISTICS MAY NEED ADJUSTING FOR THE SOMEWHAT ROUGH AND POROUS SURFACE. ONE COMBINATION OF PAINT AND SPRAYED METAL (ZINC CHROMATE PRIMERS ON SPRAYED ZINC IN A MARINE ATMOSPHERE) LED TO DEGRADATION OF THE TOP- COAT PAINT AND THIS COMBINATION IS NOT RECOMMENDED. ON THE WHOLE, THE PAINTED METAL-SPRAYED COATINGS EXPOSED AT BOTH SITES (INDUSTRIAL AND MARINE ATMOSPHERES) ARE STILL IN SATISFACTORY CONDITION AND THE TESTS ARE CONTINUING. THE FORMULATIONS OF THE EXPERIMENTAL PRIMING PAINTS ARE GIVEN. /AUTHOR/

  • Supplemental Notes:
    • Vol 1, No 5, PP 171-180, 4 FIG, 5 TAB, 6 REF, 1 APP
  • Authors:
    • Stanners, J F
    • Watkins, K O
  • Publication Date: 1966

Media Info

Subject/Index Terms

Filing Info

  • Accession Number: 00216319
  • Record Type: Publication
  • Files: TRIS
  • Created Date: Aug 12 1970 12:00AM