SAFE HOT-STORAGE TIME EXTENDED WITH SILICONE AND INERT GAS
DETAILS ARE GIVEN OF A STORAGE METHOD OF LENGTHENING THE SAFE HOT RETENTION PERIOD FOR HOT-COATED MATERIALS WITHOUT ANY DANGER OF DETERIORATION. THE METHOD CONSISTS OF USING AN INERT GAS BLANKET OR ADDING SILICONE TO THE MIX. METHODS OF HEATING SILOS ARE REVIEWED TOGETHER WITH VARIOUS TECHNIQUES FOR ELIMINATING SEGREGATION. /LCPC/RRL/
-
Supplemental Notes:
- Vol 3, No 7, PP 83-89, 8 FIG, 3 RAB, 1 PHOT, 5 REF
-
Authors:
- Don, BROCK J
- Cox, R B
- Publication Date: 1968-7
Media Info
-
Serial:
- Roads and Streets
- Publisher: Donnelley (Reuben H) Corporation
Subject/Index Terms
- TRT Terms: Handling and storage; Hot coated materials; Methodology; Mixtures; Noble gases; Safety; Silicones; Silos; Storage facilities; Time
- Uncontrolled Terms: Segregation
- Subject Areas: Construction; Freight Transportation; Highways; Safety and Human Factors; Terminals and Facilities;
Filing Info
- Accession Number: 00214955
- Record Type: Publication
- Source Agency: Road Research Laboratory /UK
- Files: TRIS
- Created Date: Jun 1 1971 12:00AM