INCREASING THE DURABILITY OF CONCRETE BY MEANS OF ALUMINUM-METHYL-SODIUM SILICATE
POVYSHENIE DOLGOVECHNOSTI BETONA ALYUMOMETILSILIKATOM NATRIYA
The results presented demonstrate that the addition of a plasticizer (in an aqueous solution containing 33% of dry material), at the rate of 0.1 to 0.3% by weight of cement permits a reduction in the proportion of cement and of water (up to 10%), an improvement in workability, without strength of 10 to 90% with or without steam-curing. An explanation is given of the action of the plasticizer (water repellant, non-air entraining). /TRRL/
-
Corporate Authors:
Mezhdunarodnaya Kniga
Smolenskaya Sennaya Pl 32/34
Moscow G-200, USSR -
Authors:
- Piskarev, V A
- Publication Date: 1974
Language
- Russian
Media Info
- Features: References; Tables;
- Pagination: p. 31-32
-
Serial:
- Stroitel Nye Materialy
- Issue Number: 8
Subject/Index Terms
- TRT Terms: Aluminum compounds; Concrete; Concrete curing; Durability; Mix design; Plasticizers; Sodium silicate; Steam curing; Strength of materials; Water cement ratio; Workability
- Old TRIS Terms: Plasticizer (Concrete)
- ITRD Terms: 4736: Admixture; 7168: Aluminium; 4755: Concrete; 5914: Hardness; 5939: Hydrophobic; 4725: Plasticizer; 7417: Silicone; 7197: Sodium
- Subject Areas: Highways; Materials; Planning and Forecasting; I32: Concrete; I72: Traffic and Transport Planning;
Filing Info
- Accession Number: 00149672
- Record Type: Publication
- Source Agency: Central Laboratory of Bridges & Highways, France
- Report/Paper Numbers: Analytic
- Files: ITRD, TRIS
- Created Date: Aug 4 1977 12:00AM