UTILISATION DES EXSUDATS COMME INDICATEURS PRIMAIRES DE DEGRADATION DES BETONS ET MACONNERIES D'OUVRAGES D'ART

LA PRESENCE D'EXSUDATS (STALACTITES, CONCRETIONS, EFFLORESCENCES) SUR UN OUVRAGE RESULTE DE LA CIRCULATION D'EAU AU SEIN DU MATERIAU (BETON OU MACONNERIE). LA RECUPERATION DES EXSUDATS EST FACILE ET NE MUTILE PAS L'OUVRAGE. L'ANALYSE DE LEURS CONSTITUANTS (GENERALEMENT DU CARBONATE DE CALCIUM, SOUVENT ACCOMPAGNE D'AUTRES SELS) EST DESTINEE A TENTER DE DETERMINER LA NATURE ET LE DEGRE D'AVANCEMENT DE L'ALTERATION SUBIE PAR LE MATERIAU. APRES UN RAPPEL DU MECANISME DE FORMATION DES STALACTITES, L'ARTICLE MONTRE, AU MOYEN D'UNE DIZAINE D'EXEMPLES BIEN CARACTERISTIQUES, LA VARIETE DES CAUSES DE DEGRADATION DETECTEES A TRAVERS LES EXSUDATS. ON DISTINGUE : - LES EXSUDATS EXCLUSIVEMENT CALCAIRES, EN SEPARANT LE CAS OU CE CALCAIRE NE PEUT PROVENIR QUE DE LA DISSOLUTION DU LIANT DE CELUI OU IL PEUT PROVENIR SOIT DE LA DISSOLUTION DU LIANT, SOIT DE CELLE DES GRANULATS, SOIT DES DEUX ; - LES EXSUDATS PRINCIPALEMENT MAIS NON EXCLUSIVEMENT CALCAIRES : DONT LES AUTRES CONSTITUANTS PERMETTENT DE DETECTER DIVERS MECANISMES DE DEGRADATION TELS QUE REACTION ALCALI-GRANULATS, ATTAQUE SULFATIQUE, CARBONATATION ALCALINE DES ALUMINATES ; - LES EXSUDATS A CALCAIRE MINORITAIRE OU SANS CALCAIRE, QUI TRADUISENT DES DEGRADATIONS TRES VARIEES COMME LA FORMATION DE ROUILLE PROVENANT DU LESSIVAGE DU TERRAIN OU DE LA CORROSION DES ARMATURES, DES AGRESSIONS SULFATIQUES, DES ATTAQUES PAR DES PRODUITS DIVERS EMPLOYES SUR L'OUVRAGE (FONDANTS CHIMIQUES, DESHERBANTS, PAR EXEMPLE). (A).

  • Availability:
  • Authors:
    • DELOYE, F -
    • MAIRE, G
    • BUISSON, M -
  • Publication Date: 1983-3

Language

  • French

Media Info

Subject/Index Terms

Filing Info

  • Accession Number: 01278000
  • Record Type: Publication
  • Source Agency: Institut Francais des Sciences et Technologies des Transports, de l'Aménagement et des Réseaux (IFSTTAR)
  • Files: ITRD
  • Created Date: Nov 20 2010 7:09PM